Can combined attack of concentrated bromate ions and thermal cycling cause passivation layer spalling and subsurface corrosion of titanium heating tubes?

Nov 16, 2026

Leave a message

Titanium heating components are widely used in bromate-containing oxidation baths and water treatment reaction systems. Most compatibility data focuses on static immersion at stable temperature, while the synergistic hazard of bromate reduction and thermal cycling is rarely documented. Bromate is a strong oxidising ion. When it contacts the titanium oxide film, reduction reactions occur at the oxide interface, generating reactive oxygen species. These reactive species introduce internal stress into the TiO₂ passive film. Repeated heating and cooling adds thermal mismatch stress, creating microcracks that propagate through the oxide layer. Once cracks form, bromate ions penetrate to the fresh metal surface and trigger new oxidation cycles. Instead of uniform thinning, the oxide film flakes off in layered fragments. New passive film repeatedly forms and spalls, leading to progressive subsurface metal loss. Weld zones are more vulnerable because their oxide films are inherently heterogeneous and carry residual welding stress.

The degradation pathway consists of oxidant-induced internal stress, thermal crack generation and cyclic film spalling. Bromate reduction consumes electrons at the metal-oxide interface, changing the stoichiometry of titanium oxide and building compressive stress inside the film. Thermal cycling expands and contracts the substrate and oxide at different rates, opening microcracks. The cracks provide fast diffusion channels for bromate. When the oxide layer detaches, bare titanium is exposed, rapidly re-oxidising to form a new but defective oxide. This cycle repeats continuously, leading to layered material loss. Higher bromate concentration and larger temperature swing both accelerate spalling.

Initial signs include patchy dark grey or black oxide scales that peel off easily when wiped. Operators often mistake loose oxide for normal oxide scaling and simply clean the surface without stopping the degradation process.

表格

Stage Surface Feature Metallurgical State Risk Level Recommended Action
Bromate adsorption and oxide stress build-up Uniform dark tint, oxide adheres tightly Internal stress accumulates within TiO₂ film Low Reduce bromate concentration; stabilise bath temperature
Oxide microcrack formation Fine fissures visible under magnification Cracks penetrate oxide layer, ion diffusion pathways open Medium Reduce temperature fluctuation; add reducing agents if process allows
Layered spalling and subsurface etching Loose oxide flakes, rough fresh metal areas Cyclic oxide formation and detachment High Remove heater for inspection; use dye penetrant testing
Severe thinning and cracking Deep localised metal loss, structural cracks Cross-sectional thickness reduced below safe threshold Critical Replace heater; switch to PFA coated heating assemblies

Preventive measures focus on bromate concentration control and thermal stabilisation. Adjust upstream treatment processes to reduce incoming bromate loading. Keep bath temperature stable and avoid rapid heating and quenching. Where bromate cannot be removed, relocate heaters outside the high-bromate reaction zone or select fluoropolymer coatings. Stress relief after welding reduces residual stress in weld heat-affected zones.

XPS surface analysis can identify reduced bromine species on titanium surfaces. A common error is assuming titanium's oxidation resistance works equally well under cyclic oxidising bromate exposure. In summary, bromate generates stress within the titanium passive film, and thermal cycling drives cracking and spalling, so oxidant control and temperature stabilisation are critical.

info-717-483

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.