Can combined attack of oxidising bromide species and thermal cycling cause selective grain boundary corrosion of titanium heating tubes?

Nov 16, 2026

Leave a message

Titanium heating tubes are commonly used in bromide-containing reaction systems, seawater related processes and bromine regeneration baths. It is widely accepted that titanium performs well in bromide solution under ambient temperature, yet the synergistic effect of oxidising bromine species and repeated thermal cycling is often underestimated. Oxidising bromide species including Br₂, BrO⁻ and tribromide ions can break the continuity of titanium dioxide passive film. Thermal cycling introduces alternating tensile and compressive stress on the oxide layer, generating microcracks along grain boundaries. Oxidising bromide species penetrate these cracks and attack grain boundaries preferentially. The grain boundary region has higher energy and contains more segregated impurities, so it dissolves faster than the grain matrix. This failure mode manifests as grain boundary loosening and intergranular spalling, rather than uniform pitting corrosion. Even if the overall metal loss rate is low, the bonding between grains gradually weakens, bringing risk of brittle fracture under thermal or mechanical load.

The degradation mechanism combines passive film cracking by thermal stress and selective grain boundary dissolution by oxidising bromine species. Titanium forms a protective TiO₂ film when exposed to aqueous environments. However, thermal cycling creates mismatch strain between the oxide film and metal substrate, initiating microcracks. Oxidising bromine species migrate through crack channels and reach fresh grain boundaries. Impurity segregation at grain boundaries reduces local corrosion resistance, and selective dissolution occurs. As grain boundaries are etched away, individual grains lose intergranular bonding. Repeated heating and cooling cycles continuously open new crack paths for bromine species ingress. Weld heat-affected zones are the most vulnerable locations due to altered grain structure and higher residual stress.

Initial symptoms include dull, matte surface discoloration and fine powdery corrosion residues. Operators often mistake this for normal surface oxidation of titanium at high temperature.

表格

Stage Surface Feature Metallurgical State Risk Level Recommended Action
Oxidising bromide adsorption and film microcrack initiation Slight darkening of surface, no obvious grain loss Oxide microcracks form under thermal stress Low Reduce bromine concentration; stabilise bath temperature
Grain boundary selective etching Matte surface, fine grey corrosion powder Bromine species attack grain boundaries preferentially Medium Limit temperature fluctuation; add reducing agent if process permits
Grain loosening and intergranular spalling Rough surface with loose grains falling off Grain boundary network is severely etched High Take heater offline; perform metallographic inspection
Intergranular fracture and failure Fragmentation along grain boundaries, structural collapse Intergranular cohesion completely lost Critical Replace heater; switch to fluoropolymer coated heating elements

Preventive measures focus on controlling oxidising bromine concentration and reducing thermal cycling. Stabilise bath temperature to minimise rapid temperature swings. Adjust process redox potential to reduce the concentration of elemental bromine and hypobromite. Optimise welding process and carry out post-weld stress relief to reduce residual stress in weld zones. Where oxidising bromide cannot be eliminated, fully PFA coated heaters are preferred.

Scanning electron microscopy with grain boundary mapping can confirm intergranular corrosion. A common error is extending titanium's good static bromide resistance to dynamically cycled thermal environments. In summary, oxidising bromine species penetrate thermally induced oxide cracks and selectively corrode grain boundaries of titanium, and redox control and temperature stabilisation are key safeguards.