Can iodine species adsorption and iodine-induced oxide embrittlement trigger spalling corrosion of titanium heating tubes in iodine-containing wet scrubber systems?

Nov 16, 2026

Leave a message

Titanium heating elements are widely used in wet scrubbers, iodine recovery and halogen waste treatment systems. Engineers generally trust titanium's resistance to dilute iodine solutions at room temperature. However, in wet gaseous scrubber environments, molecular iodine, iodide ions and triiodide complexes coexist and repeatedly adsorb onto the titanium oxide surface. Iodine species penetrate the oxide lattice and alter the stoichiometry of TiO₂, making the passive film brittle. Under thermal cycling stress, the brittle oxide layer cracks and flakes off. Fresh titanium substrate is exposed and immediately reacts with iodine species to form titanium iodide compounds. These iodides are unstable in aqueous conditions and hydrolyse quickly, leaving a defective new oxide layer. The cycle of oxide formation, iodine penetration, embrittlement and spalling repeats continuously. Unlike uniform pitting, this failure shows layered peeling of the surface, and weld heat-affected zones degrade first due to non-uniform oxide structure.

The degradation mechanism includes iodine lattice incorporation, oxide embrittlement and thermally driven film spalling. Iodine atoms penetrate the TiO₂ passive film and occupy interstitial lattice positions, introducing internal residual stress. The modified oxide loses its original ductility and becomes brittle. Thermal cycling creates strain mismatch between oxide and metal substrate, opening cracks across the iodine-contaminated oxide. Once cracks reach the metal interface, iodine species contact fresh titanium and form unstable titanium iodides. Subsequent hydrolysis generates oxide and releases iodine back into the system, allowing the cycle to continue. Higher temperature increases iodine diffusion rate and hydrolysis speed.

Initial symptoms include patchy brown, purple and grey mottled discoloration on the surface. Operators often regard these colourful stains as normal thermal oxidation tinting.

表格

Stage Surface Feature Metallurgical State Risk Level Recommended Action
Iodine adsorption and lattice incorporation Iridescent brown-purple mottled tint, oxide adheres tightly Iodine enters oxide lattice, internal stress accumulates Low Reduce iodine loading; improve gas-liquid separation
Oxide embrittlement and microcrack generation Fine fissures visible under magnification Brittle oxide develops crack networks Medium Stabilise temperature; reduce thermal cycling frequency
Layered spalling and cyclic hydrolysis Loose oxide flakes, rough fresh metal exposed Repeated oxide loss and reformation High Remove heater; conduct dye penetrant inspection
Severe metal thinning and cracking Deep corroded zones, structural cracks Cross-section thickness drops below safe limit Critical Replace heater; switch to PFA coated heating components

Preventive measures focus on iodine containment and thermal stabilisation. Install mist eliminators to reduce iodine-laden droplets reaching the heater. Adjust solution redox state to convert elemental iodine into less aggressive iodate forms where process permits. Reduce temperature swing amplitude and avoid thermal shock. For high iodine environments, fluoropolymer coated heaters are a more reliable alternative.

XPS surface analysis can detect iodine trapped within the oxide layer. A common error is extrapolating titanium's stability in dilute static iodide solution to wet iodine vapour scrubber conditions. In summary, iodine species infiltrate titanium passive film and induce oxide embrittlement, and thermal cycling drives continuous spalling, so iodine vapour control is essential.