Can sulphate reducing bacteria (SRB) biofilm and acid generation induce under-deposit pitting corrosion of duplex stainless steel heating tubes in closed recirculating process water?

Nov 17, 2026

Leave a message

Duplex stainless steel, characterised by balanced austenite and ferrite phases, is widely adopted for heating tubes in process water loops, cooling circuits and low-chloride industrial tanks due to its superior strength and pitting resistance compared with conventional 316 stainless steel. Plant designers often rely on its high PREN (Pitting Resistance Equivalent Number) value and assume the alloy is immune to microbial corrosion, yet this assumption overlooks the destructive under-deposit corrosion triggered by sulphate reducing bacteria. SRB are anaerobic microorganisms that thrive beneath slime deposits, sludge and inorganic scales on heater surfaces. While the bulk water maintains neutral pH and acceptable water quality, the microenvironment trapped under the biofilm becomes entirely different. SRB consume sulphate ions in the water and produce hydrogen sulphide as a metabolic by-product. Hydrogen sulphide dissociates to form bisulphide and sulphide ions, which break down the passive chromium oxide film on duplex stainless steel. In addition, the metabolic activity of the biofilm creates oxygen concentration cells: the area under the deposit is oxygen-depleted and acts as an anode, while the surrounding clean surface serves as the cathode. The combination of sulphide chemical attack and differential aeration drives localised pitting, which can penetrate the tube wall far faster than general corrosion. Unlike uniform corrosion, microbial pitting is highly localised, and pits tend to form at phase boundaries between ferrite and austenite, as the two phases have slight electrochemical potential differences that further accelerate pit propagation.

The core mechanism lies in the formation of a self-sustaining aggressive microclimate under biofilm. A mature biofilm is not just a thin layer of slime; it is a porous composite of extracellular polymeric substances, trapped mineral particles and microbial colonies. It blocks oxygen diffusion, establishing anaerobic conditions ideal for SRB. Sulphate reduction produces H₂S, which reacts with the passive oxide film to form thin, non-protective iron sulphide layers. Iron sulphide is electronically conductive, and it functions as an efficient cathode, accelerating the dissolution of the adjacent metal substrate. Duplex steel's dual-phase microstructure introduces galvanic coupling between ferrite and austenite. Ferrite is preferentially attacked in sulphide-rich environments, so pits initiate selectively within ferrite domains or along phase boundaries. As the pit deepens, corrosion products accumulate inside the cavity, further restricting mass exchange and stabilising the low-pH, sulphide-rich environment. This positive feedback loop allows pits to grow continuously even when the bulk water chemistry is kept within specification limits. Thermal cycling of the heater worsens the situation: temperature fluctuations expand and contract the biofilm, creating microcracks that allow fresh nutrients and sulphate to penetrate deeper, while the heated surface provides an optimum temperature range for SRB reproduction.

Early signs are subtle and easy to overlook. A thin, grey-black slimy deposit adheres to the low-flow zones and liquid line of the heating tube. After wiping away the slime, tiny dark pits or etched patches appear on the metal surface. Operators often classify these deposits as ordinary dirt and remove them with simple water flushing, which fails to eliminate embedded microbial colonies and does not repair the damaged passive film.

表格

Stage Surface Feature Electrochemical & Metallurgical State Risk Level Recommended Action
Biofilm colonisation Thin translucent slime, no visible metal damage SRB adheres to surface, oxygen gradient begins Low Implement regular biocide dosing and flow velocity optimisation
Sulphide generation and film breakdown Grey-black sticky deposit, faint discoloration under slime H₂S accumulates, passive oxide film locally degraded Medium Perform online biofilm monitoring; adjust biocide type and frequency
Pit initiation along phase boundaries Discrete tiny pits, sulphide corrosion products inside pits Ferrite phase preferentially dissolves, local anode forms High Isolate heater for inspection; conduct pit depth measurement
Pit penetration and leakage Through-wall perforation, process fluid leakage Pit breaches tube wall, containment failure Critical Replace heater; redesign water treatment and monitoring scheme

Mitigation strategies target biofilm suppression and sulphide formation. Maintaining sufficient flow velocity prevents sludge settlement and limits biofilm attachment. Combined biocide programmes, alternating oxidising and non-oxidising biocides, avoid SRB developing drug resistance. Periodic pigging or chemical cleaning removes mature deposits, but cleaning agents must be compatible with duplex stainless steel to avoid introducing extra corrosion. Online monitoring of sulphide concentration, oxidation-reduction potential and adenosine triphosphate (ATP) provides early warning of microbial activity. It is also necessary to avoid long-term stagnation during equipment shutdown, because static water is the most favourable condition for SRB proliferation.

Metallographic examination and energy dispersive spectroscopy can detect sulphide residues inside pits and confirm microbial corrosion. A widespread misconception is that high PREN alloys are inherently resistant to all pitting forms. PREN only predicts resistance to chloride pitting, not sulphide-induced microbial attack. In summary, SRB biofilm creates anaerobic microzones, hydrogen sulphide destroys passivation, and duplex phase boundaries become preferential pitting sites, so integrated water quality and microbial control are indispensable.

 

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!