Can alkaline transgranular stress corrosion cracking of alloy 20 heating tubes occur in hot phosphate-containing process liquors?

Nov 17, 2026

Leave a message

Alloy 20, also known as Carpenter 20, is widely selected for heating tubes in phosphoric acid production, phosphate fertilizer processing and neutralised alkaline phosphate circuits, valued for its excellent resistance to sulphuric acid and general acid corrosion. Many process engineers regard Alloy 20 as a reliable universal choice for mixed phosphate and alkaline service, assuming its high nickel and chromium content provides immunity to stress corrosion cracking. This assumption overlooks the specific risk of transgranular stress corrosion cracking triggered by hot phosphate-alkali mixed environments. When phosphate and free hydroxide coexist at elevated temperatures, a reactive local environment forms at the metal surface, especially at areas with residual tensile stress from welding, bending and tube rolling. Unlike chloride-induced cracking which is more familiar to maintenance teams, phosphate alkaline cracking propagates along transgranular paths, leaving few obvious corrosion deposits on the fracture surface. The passive nickel-chromium oxide film becomes unstable under combined high temperature and phosphate complexation. The film locally dissolves, and the crack tip remains electrochemically active. Even with low measurable general corrosion rates, sharp cracks can penetrate the tube wall, leading to sudden leakage. This failure is often misattributed to thermal fatigue, because the fracture surface is clean and lacks thick corrosion scales.

The core mechanism relies on phosphate complexation of chromium and sustained anodic dissolution at crack tips. In hot alkaline phosphate solutions, phosphate anions form soluble chromium-phosphate complexes, removing chromium from the protective oxide layer. The oxide film cannot re-passivate rapidly once locally damaged. Tensile stress continuously opens the crack mouth, exposing fresh metal at the crack tip while the surrounding surface stays passive and acts as the cathode. The electrochemical driving force concentrates dissolution within a narrow crack tip zone. The crack grows transgranularly through the alloy grains rather than along grain boundaries, which distinguishes it from intergranular sensitisation cracking. Residual stress from fabrication is the primary accelerating factor. Heater zones close to welds, bends and flanged connections are the most vulnerable. Boiling and localised surface evaporation concentrate phosphate and hydroxide ions into a thin boundary film, making the surface chemistry far more aggressive than the bulk solution sampled by operators. Thermal cycling amplifies tensile stress, opening microcracks and allowing electrolyte to penetrate deeper.

Early warning signs are subtle. The tube surface may show faint pale grey phosphate staining, and no obvious pits or thinning can be detected by thickness measurement. Penetrant testing is usually required to reveal fine hairline cracks.

表格

Stage Surface Feature Electrochemical & Metallurgical State Risk Level Recommended Action
Boundary layer concentration Faint pale grey staining, intact surface Phosphate and hydroxide concentrate at heated surface, film starts thinning Low Control bulk temperature; avoid surface boiling
Local film breakdown at stress raisers No visible cracks, staining concentrated at weld toes Chromium complexation breaks passivity, crack nuclei form Medium Post-weld stress relief; reduce local hot spots
Transgranular crack extension Fine hairline cracks visible under penetrant Crack tip dissolution continues, transgranular path develops High Isolate heater; suspend continuous operation
Through-wall penetration Clean fracture face, minimal corrosion product Crack breaches tube wall, process fluid leakage Critical Replace tube; re-evaluate alloy or operating chemistry

Mitigation begins by breaking the three prerequisites: aggressive phosphate-alkali environment, elevated temperature and tensile stress. Where process permits, reduce free hydroxide concentration and avoid boiling conditions on the heater sheath. Post-weld heat treatment to eliminate residual tensile stress is highly effective. If the service environment cannot be modified, nickel-based alloys such as Hastelloy G30 are more resistant to phosphate alkaline cracking. Regular inspection using dye penetrant and eddy current testing is necessary, as ultrasonic thickness checks cannot detect fine transgranular cracks.

A common misconception is that acid-resistant alloys automatically resist alkaline stress corrosion. Alloy 20's strong performance in sulphuric acid does not translate to immunity in hot alkaline phosphate mixtures. In summary, phosphate ions dissolve chromium oxide, tensile stress drives transgranular crack growth, and local surface concentration creates aggressive microenvironments even when bulk solution is controlled.

info-717-483

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!