Why Do Sour Gas Amine Reboilers Deposit Iron Sulfide on Metal Heaters and How Does a PTFE Immersion Heater Stop It?

Sep 14, 2026

Leave a message

The Iron Sulfide Fouling Problem

Sour gas processing uses amine solutions to absorb hydrogen sulfide from natural gas. The rich amine is regenerated in a reboiler, where the solution is heated to 120–135°C to drive off the acid gases. The reboiler immersion heater faces a persistent fouling problem: iron sulfide deposition.

The iron sulfide originates from two sources. The dissolved iron in the amine solution-from upstream corrosion of carbon steel equipment-reacts with the H₂S to form insoluble iron sulfide particles. Simultaneously, the metal heater surface corrodes in the hot amine solution, forming iron sulfide directly on the surface.

The iron sulfide deposit is black, dense, and adherent. It reduces heat transfer, provides a site for further corrosion, and requires frequent cleaning. The deposit creates a microenvironment under which corrosion accelerates-a phenomenon known as under-deposit corrosion.

A PTFE immersion heater stops the iron sulfide deposition through multiple mechanisms.

Why Iron Sulfide Bonds to Metal Surfaces

On a carbon steel or stainless steel heater surface in sour amine service, two processes occur simultaneously.

The metal surface corrodes in the amine solution. The corrosion reaction produces iron ions at the surface. These iron ions immediately react with the dissolved H₂S to form iron sulfide:

Fe²⁺ + H₂S → FeS + 2H⁺

The iron sulfide precipitates directly on the metal surface where the iron ions were generated. The deposit is chemically bonded to the metal-it is a corrosion product, not a separate deposit.

The bulk iron sulfide particles-formed when dissolved iron in the amine reacts with H₂S-also deposit on the heater surface. These particles adhere to the existing corrosion product layer.

A PTFE immersion heater has no iron to corrode. There is no surface corrosion product. The iron sulfide particles that precipitate from the bulk amine contact an inert surface that offers no chemical bonding and minimal adhesion.

Table 1: Iron Sulfide Fouling on Heater Materials in Amine Service

Material Surface Corrosion FeS Formation on Surface Particle Adhesion Cleaning Method Service Life
Carbon Steel Yes Yes (corrosion product) Strong Mechanical/acid 6–12 months
Stainless Steel 316L Slow Yes (thinner layer) Moderate Mechanical/acid 12–24 months
PTFE Immersion Heater None None Very weak Water rinse 10+ years

Service life from refinery amine unit maintenance records.

The PTFE Advantage: No Corrosion, No Catalysis

PTFE has no metal to corrode. There is no iron source for the iron sulfide formation. The surface does not participate in the corrosion reaction that generates FeS directly on the heater.

The PTFE surface is also non-catalytic. The metal oxide surface can catalyze the oxidation of amine degradation products, which contribute to fouling. PTFE does not promote these reactions.

The Under-Deposit Corrosion Elimination

Iron sulfide scale on metal surfaces creates under-deposit corrosion. The scale blocks the diffusion of oxygen and treatment chemicals to the metal surface. The trapped environment becomes acidic and aggressive. Pitting initiates under the scale and propagates rapidly.

A PTFE immersion heater eliminates under-deposit corrosion by eliminating the surface scale layer. Without an adherent scale, there is no occluded zone for under-deposit attack.

Field Experience at a Refinery Amine Unit

A refinery amine regeneration unit operated a reboiler with carbon steel immersion heaters. The heaters developed an iron sulfide scale within four weeks. The scale reduced heat transfer by 35% and required mechanical cleaning every month. The cleaning involved draining the reboiler, scraping the deposits, and acid washing.

The refinery replaced the carbon steel heater with a PTFE immersion heater. After 18 months of operation, the PTFE surface showed only a light, powdery deposit that was removed by a water rinse during the annual turnaround. The heat transfer coefficient remained stable. The cleaning frequency dropped from monthly to annually. The maintenance cost decreased by 80%.

Summary

Iron sulfide deposits on metal immersion heaters in sour gas amine reboilers through surface corrosion and particle adhesion. The deposit reduces heat transfer and causes under-deposit corrosion. A PTFE immersion heater eliminates the corrosion source and resists particle adhesion.

For refineries and gas processing plants, a PTFE immersion heater provides a reliable, low-maintenance heating solution in amine reboiler service. Custom sizing based on amine composition, reboiler duty, and steam conditions can be provided upon submission of the process parameters.