What Is the Impact of Long-time Static Immersion on PFA Anti-corrosion Heating Tubes?

Sep 19, 2026

Leave a message

PFA anti-corrosion heating tube uses seamless PFA fluoroplastic coating to wrap the metal heating core. PFA, perfluoroalkoxy polymer, is a high-performance fluoropolymer with broad-spectrum chemical resistance. It can resist most strong acids, strong alkalis, oxidants and organic solvents. The intact PFA coating completely separates the internal metal heating element from corrosive liquid and avoids metal corrosion.

PFA coating has non-stick surface characteristics, and chemical deposits are difficult to accumulate. But static long-term immersion in some strong chemical media will bring hidden risks. Even without scratches, some high-purity corrosive agents may slowly penetrate the coating over months, forming blisters between coating and metal substrate. Meanwhile, PFA has a

coating easily.

The table shows static immersion test results of PFA coating in different chemicals:

表格

Immersion Medium Concentration Temperature Coating Condition after 6 months
Nitric acid 20% 60℃ No visible change
Sodium hydroxide 30% 70℃ Slight swelling
Organic solvent (acetone) Pure 50℃ Stable
Hot concentrated chromic acid 25% 90℃ Minor blistering

PFA heating tubes are widely used in semiconductor wet treatment, fine chemical reaction tanks and chemical wastewater treatment. Before putting into service, static immersion tests can be conducted to verify coating adaptability. Operators need to inspect coating surface for blisters and peeling regularly. For low and medium temperature, static or slowly flowing mixed corrosive liquid, PFA heating tubes provide stable anti-corrosion heating performance under proper monitoring

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.