Persulfate-Induced Localized Pitting of Titanium Immersion Heaters in Copper-Board Etching Regeneration Baths

Sep 05, 2026

Leave a message

Titanium immersion heaters are used in copper-board etching and etchant regeneration lines where persulfate-based oxidizers are applied. Persulfate is a powerful oxidizing agent that is stable at moderate temperature but can decompose at heated titanium surfaces, generating sulfate radicals and oxygen. These reactive species can locally disrupt the titanium dioxide passive film. When chloride, present as an etchant by-product, coexists, it penetrates the weakened film and initiates pitting. This failure mode is often overlooked because titanium is generally considered highly resistant to persulfate oxidizers.

The degradation mechanism involves radical attack and film destabilization. At heated sheath surfaces, persulfate decomposition produces sulfate radicals that react with the TiO₂ layer, causing local thinning and defect formation. Chloride ions then migrate into these defects and stabilize pit cavities. Once pitting starts, the radical-rich local environment prevents repassivation. Damage concentrates at high-temperature zones and bubble-release sites where persulfate decomposition is most intense.

Early-stage signs include dull surface patches, loss of metallic luster and scattered micro-pits after cleaning. Operators may attribute these signs to etchant contamination. Preventive measures include limiting persulfate concentration in heating zones, controlling sheath temperature to reduce decomposition rate, optimizing bath circulation, and inspecting high-temperature zones for hidden pitting.

表格

Etchant Bath Condition Persulfate Pitting Risk Core Degradation Mechanism Early-stage Feature Core Control Strategy
Persulfate etchant with chloride and heating High Persulfate decomposes to sulfate radicals; TiO₂ film thins and develops defects; chloride initiates and stabilizes pits Dull patches; loss of luster; scattered micro-pits after cleaning Limit persulfate near heaters; control sheath temperature; improve circulation; high-temperature zone inspection
Persulfate-free stable etchant Low Titanium passive film remains stable; no radical-induced defect formation Bright metallic surface without pitting Maintain controlled etchant chemistry and temperature

Conclusion: Persulfate decomposition at heated titanium surfaces can cause hidden localized pitting. Oxidizer concentration and sheath temperature control are critical in copper-board etching regeneration baths.

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!