Can phosphate glassy scale and thermal shock fatigue induce crack growth of quartz anti-corrosion heating tubes?

Nov 15, 2026

Leave a message

Fused quartz heating tubes are widely used in phosphoric acid concentration and phosphate chemical treatment systems, praised for excellent resistance to most mineral acids. Maintenance teams are familiar with quartz damage from strong alkali, but the synergistic failure caused by phosphate glassy scale and thermal shock fatigue is rarely recognised. When phosphoric acid concentrates on the heater surface, phosphate species precipitate into a dense, glass-like scale upon cooling. This phosphate scale has a thermal expansion coefficient drastically different from fused quartz. Each heating and cooling cycle creates large interfacial shear stress between the scale and quartz substrate. The rigid scale cannot deform together with quartz, initiating microcracks at the scale-quartz boundary. Meanwhile, hot concentrated phosphate slowly etches silica at crack tips, weakening Si-O bonds and accelerating crack extension. This combination of mechanical fatigue and chemical attack can lead to sudden fracture even under moderate temperature swings.

The synergistic degradation mechanism combines thermal expansion mismatch and local chemical etching. The glassy phosphate scale adheres tightly to quartz and cannot flex with the substrate during temperature changes. Alternating tensile and compressive stress concentrates at the interface, generating microcracks. Concentrated phosphate liquid seeps into crack tips and slowly dissolves silica. Each thermal cycle makes the crack slightly longer. The crack growth rate accelerates as cracks become larger. High heat flux zones where phosphate concentrates and precipitates are the main failure locations. Thick glassy scale is hard to remove with ordinary acid cleaning.

At the early stage, a translucent pale grey glassy layer covers the quartz surface, and the underlying quartz remains transparent, so operators ignore the hidden stress risk.

The following table summarises progressive quartz tube degradation caused by phosphate glassy scale and thermal shock fatigue.

表格

Stage Surface Feature Physical and Chemical State Risk Level Recommended Action
Thin phosphate scale deposition Translucent pale grey glassy film, quartz transparent Scale adheres, minor interfacial stress builds Low Reduce acid concentration; limit surface boiling
Interfacial microcrack initiation Scale thickens, tiny hidden cracks under scale Thermal mismatch stress generates microcracks Medium Slow heating and cooling rate; use targeted phosphate cleaners
Chemically assisted crack extension Clear branching cracks across scaled regions Phosphate etches crack tips, cracks grow steadily High Stop heating; inspect cracks with optical microscopy
Thermal shock fracture Quartz splits along interconnected crack networks Crack reaches critical fracture length Critical Replace tube; redesign process to reduce phosphate precipitation

Mitigation focuses on phosphate precipitation control and gentle thermal operation. Keep bulk phosphoric acid below saturation concentration to avoid surface precipitation. Reduce heating ramp speed to lower interfacial stress. Use specialised phosphate-dissolving cleaners instead of mechanical scraping. Schedule regular cleaning before scale forms thick glassy layers.

Polarised light microscopy can detect hidden microcracks under translucent scale. Many technicians only watch for alkali corrosion and ignore phosphate scale damage. Once cracks form, chemical etching will continuously push crack growth. In summary, phosphate glassy scale creates cyclic thermal stress, while concentrated phosphate etches crack tips, and concentration control plus regular descaling are key protective measures.

info-717-483

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!