Fused quartz heating tubes are used in molten salt baths, high-temperature salt evaporation and solar thermal receiver systems, where they may come into contact with alkali or alkaline-earth salt melts. Operators are generally aware that strong alkalis can etch quartz, but the combined effect of molten salt infiltration and thermal gradient stress is less often recognised. When molten salt enters surface microcracks or grain boundary-like defect networks in quartz, it can remain trapped during cooling. On reheating, the salt remelts and expands, generating internal pressure inside the defects. Thermal gradients across the quartz tube add additional mechanical stress, causing cracks to extend slowly. This is not simply chemical dissolution; it is a synergistic process in which molten salt acts as both a chemical agent and a mechanical wedge. Damage often accumulates beneath the surface and may not become visible until cracks connect and cause sudden fracture.

The synergistic degradation mechanism involves molten salt capillary penetration, internal pressure generation and stress-assisted crack growth. Quartz naturally contains tiny surface flaws, grinding marks and sub-surface defects. Molten salt is drawn into these defects by capillary action. When the salt solidifies during cooling, it contracts, but on reheating it expands rapidly. If the salt remains confined, the resulting internal pressure can propagate existing cracks. Thermal gradients add tensile and shear stress, especially near hot zones and areas of rapid temperature change. Alkali ions from the molten salt can also weaken Si-O bonds at crack tips, reducing the energy required for crack extension. The process is therefore both mechanically and chemically assisted.

At an early stage, quartz may show only faint cloudy patches or discoloration near the salt contact region. These features are often mistaken for light staining or normal high-temperature haze.

The following table summarises progressive quartz tube degradation caused by molten salt infiltration and thermal gradient stress.

表格

Stage Surface Feature Physical and Chemical State Risk Level Recommended Action
Molten salt surface wetting Localised transparent or cloudy salt films, no obvious cracks Salt wets surface defects, initial capillary infiltration Low Apply protective coatings; prevent salt splashing
Salt entrapment and microcrack growth Slight subsurface haze, faint crack lines under magnification Solidifying and remelting salt generates internal stress Medium Reduce thermal gradient; slow heating and cooling rates
Crack network development Clear branching cracks, some filled with white or coloured salt Cracks extend under thermal stress and chemical weakening High Stop service; inspect crack network with polarised light microscopy
Catastrophic fracture Sudden breakage along crack networks, loss of structural integrity Crack length exceeds critical fracture threshold Critical Replace tube; isolate quartz from direct molten salt contact

Mitigation focuses on preventing molten salt ingress, reducing thermal gradients and improving surface defect quality. Use protective ceramic coatings or barrier sleeves to prevent direct contact between quartz and molten salt. Optimise heater design to reduce steep thermal gradients. Control heating and cooling rates to limit thermal stress. Polish and anneal quartz components to reduce initial surface defects. Remove salt deposits carefully before they become deeply trapped.

Polarised light microscopy and ultrasonic scanning can detect sub-surface cracks. A common oversight is attributing all quartz cracking to thermal shock alone. In summary, molten salt can infiltrate quartz defects, generate internal pressure and act with thermal gradient stress to drive sub-surface crack growth, and barrier protection and stress control are essential preventive measures.