Titanium heating tubes are widely used in many high-temperature chemical systems, trusted for stable oxide film performance in oxidising and neutral media. Engineers usually recognise titanium's weakness in hydrofluoric acid, yet corrosion triggered by residual molten fluoride salt after high-temperature processes is often overlooked. Fluoride salts can deposit on the titanium surface during heating. When temperature rises above the salt melting point, molten fluoride penetrates tiny grain boundary gaps and reacts with TiO₂ film to form soluble titanium fluoride complexes. Unlike uniform surface corrosion, the attack preferentially propagates along grain boundaries. Repeated heating and cooling cycles open grain boundaries further, allowing more molten salt to infiltrate. The exposed outer surface may remain bright, while grain boundaries are gradually dissolved, which reduces the mechanical integrity of titanium. This risk is prominent in high-temperature melting, sintering and salt-bath processing systems.

The degradation mechanism relies on molten fluoride fluxing and grain boundary penetration. Molten fluoride acts as a flux that dissolves the titanium dioxide passive film. Grain boundaries are high-energy regions with higher chemical reactivity, so corrosion proceeds preferentially along these paths. After cooling, solidified fluoride residue stays trapped inside grain boundaries. In the next heating cycle, the salt remelts and continues deepening grain boundary attack. Thermal cycling introduces alternating thermal stress, widening grain boundary gaps and accelerating salt ingress. Higher temperature increases the solubility of titanium fluoride complexes and speeds up interfacial reactions. Low oxygen concentration suppresses passive film self-repair.

Early signs are subtle. Only faint white salt residues appear on the surface, and no obvious corrosion pits are visible. Technicians often brush away salt residues and assume the heater is safe.

The following table describes the staged degradation of titanium heaters under molten fluoride salt grain boundary corrosion.

表格

Stage Surface Feature Metallurgical State Risk Level Recommended Action
Fluoride salt deposition Scattered white salt spots, oxide film intact Solid fluoride adheres, no melting or grain boundary attack Low Prevent salt splashing; clean residues immediately after shutdown
Molten salt fluxing and film breakdown Salt melts, faint dark grain boundary lines appear TiO₂ film dissolves, grain boundary attack starts Medium Reduce operating temperature below salt melting point
Intergranular channel expansion Clear etched grain boundary network visible Continuous dissolution along grain boundaries, mechanical strength drops High Stop operation; perform metallographic cross-section inspection
Intergranular cracking and leakage Cracks follow grain boundaries, wall penetration Loss of grain cohesion leads to brittle fracture Critical Replace heater; isolate titanium elements from fluoride salt baths

Preventive strategies centre on fluoride salt exclusion and temperature control. Install splash baffles to avoid fluoride salt splashing onto titanium surfaces. Keep operating temperature below the melting point of fluoride salt. After each production batch, cool the system and clean fluoride residues with compatible cleaning agents. Avoid rapid thermal cycling that widens grain boundaries.

Metallographic section analysis is the gold standard to verify intergranular corrosion. Ion chromatography tests residual fluoride content. A common error is assuming solid fluoride salt is harmless to titanium. In summary, molten fluoride salt dissolves titanium passive film and preferentially corrodes grain boundaries under thermal cycling, and splash protection plus temperature control are core protection methods.