Can high-temperature chloride eutectic salt deposition trigger intergranular corrosion of 316 stainless steel anti-corrosion heating tubes?

Nov 15, 2026

Leave a message

316 stainless steel immersion heaters are frequently deployed in high-temperature molten salt baths and concentrated brine evaporation systems, where operating temperatures often climb above 180°C. Most corrosion management focuses on free chloride ions in bulk liquid, while intergranular corrosion induced by chloride eutectic salt deposition remains a frequently overlooked failure pathway. When brine evaporates rapidly on the heater surface, chloride salts precipitate and form thin, adherent eutectic layers. These eutectic mixtures melt at relatively low temperatures and spread along grain boundaries of 316 stainless steel. The molten salt locally dissolves chromium carbides that precipitate at grain boundaries during thermal exposure, depleting chromium along grain boundaries and breaking the continuity of the protective chromium oxide passive film. Once grain boundaries become chromium-depleted, galvanic couples form between grain boundaries and intact grain interiors, and corrosion propagates along grain boundaries without obvious surface pitting. This failure mode is particularly dangerous because the surface may appear mostly intact before the tube loses mechanical strength and fractures.

The core degradation mechanism is chromium depletion along grain boundaries driven by molten chloride eutectics. At elevated service temperatures, 316 stainless steel is susceptible to carbide precipitation at grain boundaries. When molten chloride salt contacts these carbide zones, it selectively dissolves chromium-rich phases. The chromium concentration at grain boundaries drops below the threshold required to maintain passive film stability. The grain boundaries turn anodic relative to the grain body, and corrosion advances preferentially along grain boundaries. Repeated evaporation and rewetting cycles continuously replenish the chloride salt layer, sustaining the corrosive environment. Areas with high heat flux, where evaporation is fastest, are the primary sites for salt accumulation. Weld heat-affected zones are more vulnerable because welding thermal cycles already promote carbide precipitation.

Early signs are very subtle. A thin pale salt crust covers the high-heat zones, and after washing away the salt, the surface shows faint granular discoloration that maintenance workers often dismiss as trivial staining.

The following table shows the progressive failure stages of 316 stainless steel heaters caused by chloride eutectic salt intergranular corrosion.

表格

Stage Surface Feature Electrochemical & Metallurgical State Risk Level Recommended Action
Eutectic salt deposition Thin pale salt crust on high heat flux areas Salt accumulates, no grain boundary attack yet Low Control brine concentration; reduce surface evaporation rate
Chromium carbide dissolution Faint granular discoloration after salt removal Chromium at grain boundaries starts to be leached Medium Lower operating temperature; perform electrolytic descaling
Intergranular corrosion propagation Network of narrow grain boundary grooves under surface Continuous anodic dissolution along grain boundaries High Stop operation; conduct metallographic replica inspection
Intergranular cracking and rupture Brittle fracture with rough granular fracture surface Grain bonding completely destroyed, loss of structural strength Critical Replace heater; switch to stabilised stainless steel grades

Mitigation strategies centre on preventing eutectic salt buildup and reducing carbide precipitation. Adjust process parameters to avoid surface boiling and rapid salt precipitation. Use periodic low-temperature rinsing to dissolve salt deposits before thick layers form. For high-temperature brine systems, stabilised stainless steel such as 316L is preferred to minimise carbide precipitation. Avoid excessive welding heat input and apply post-weld heat treatment where practical.

Metallographic replication and electrochemical potentiokinetic reactivation testing can detect early intergranular corrosion. Ultrasonic thickness testing is ineffective at identifying this damage because metal loss is concentrated along narrow grain boundaries. A widespread misconception is that only dissolved chloride ions cause corrosion. In summary, molten chloride eutectic salts selectively attack chromium-depleted grain boundaries of 316 stainless steel, and controlling salt deposition is the core protective measure.

info-717-483

Send Inquiry
Contact usif have any question

You can either contact us via phone, email or online form below. Our specialist will contact you back shortly.

Contact now!